Reflection 5-0
New member
After my first application with Cquartz UK, I had high spots that need to be corrected. I phoned a friend who has a reputable detail shop and works with dealer only ceramic coatings for any tips and tricks. He recommended soaking a mf towel in plain water and after the flashing period, wring the towel and wipe the solvent, place the towel immediately back into the water and wipe with a dry mf towel to pull up the water and follow up with a low nap mf towel to buff clear. This goes against anything I have ever heard or read, but tried it. To my surprise it worked! My second application went flawless and much easier with no haze or high spots. I applied a second coat with a new bucket of clean water and towel. After letting the coating cure, it seemed hydrophobic and looked amazing. Another thing I noticed, when wiping with the damp towel, it was already repelling the water and wiped clean very easy.
Has anyone else heard of this or have a different recommendation?
Has anyone else heard of this or have a different recommendation?